Point defects and primary radiation damage in Co-free Fe-Ni-Cr-Mn high-entropy alloys from molecular dynamics

Co-free Fe-Ni-Cr-Mn high-entropy alloys (HEAs) are candidates for nuclear structural applications. We used molecular dynamics with the EAM-21 potential, stiffened at short range, to study five HEAs that have been irradiated experimentally: Fe37Ni34Cr16Mn13 (ES1), Fe35Ni35Cr15Mn15 (P35), Fe46Ni22Cr15Mn17 (Y3), Fe27Ni28Cr18Mn27 (Kumar) and Fe30Ni30Cr10Mn30 (C30). They were compared with pure Ni, Fe60Ni40, the Fe70Ni10Cr20 model alloy of 316L, and Fe50Ni34Cr16, which is ES1 with Mn replaced by Fe. We calculated stacking fault energies, threshold displacement energies, point-defect formation and migration energies, and 1015 displacement cascades from 5 to 40 keV at 300 and 823 K. The stacking fault energy follows the Ni content: 19-44 mJ/m^2 in the alloys and 113 mJ/m^2 in Ni. Compared with the Mn-free alloys, the HEAs have lower threshold displacement energies (48-56 against 64-74 eV) and lower dumbbell formation energies, and Mn is the element most transported by interstitials. All the concentrated alloys leave about the same number of Frenkel pairs, 56-72 at 40 keV, half the number in Ni. At 40 keV, 54-58% of the interstitials are in clusters in the HEAs, against 67-71% in Fe60Ni40, Fe70Ni10Cr20 and Fe50Ni34Cr16 and 82% in Ni. At the same cluster size, clusters of 4-12 interstitials are faulted about half as often in the HEAs, and this does not follow the stacking fault energy. The surviving interstitials are enriched in Mn in the HEAs and in Ni in the Mn-free alloys, and depleted in Cr. The results support direct loop formation in cascades in Fe60Ni40 and Fe70Ni10Cr20 and less of it in ES1.

cond-mat.mtrl-sci↗

Atomistic Investigation of Elementary Dislocation Properties Influencing Mechanical Behaviour of $Cr_{15}Fe_{46}Mn_{17}Ni_{22}$ alloy and $Cr_{20}Fe_{70}Ni_{10}$ alloy

In this work, molecular dynamics (MD) simulations were used to investigate elementary dislocation properties in a Co-free high entropy (HEA) model alloy ($Cr_{15}Fe_{46}Mn_{17}Ni_{22}$ at. %) in comparison with a model alloy representative of Austenitic Stainless Steel (ASS) ($Cr_{20}Fe_{70}Ni_{10}$ at. %). Recently developed embedded-atom method (EAM) potentials were used to describe the atomic interactions in the alloys. Molecular Statics (MS) calculations were used to study the dislocation properties in terms of local stacking fault energy (SFE), dissociation distance while MD was used to investigate the dissociation distance under applied shear stress as a function of temperature and strain rate. It was shown that higher critical stress is required to move dislocations in the HEA alloy compared with the ASS model alloy. The theoretical investigation of simulation results of the dislocation mobility shows that a simple constitutive mobility law allows to predict dislocation velocity in both alloys over three orders of magnitude, covering the phonon drag regime and the thermally activated regime induced by dislocation unpinning from local hard configurations.

physics.atm-clus↗

Development of a Plasticity-oriented Interatomic Potential for CrFeMnNi High Entropy Alloys

An interatomic potential (termed EAM-21) has been developed with the embedded atomic method (EAM) for CrFeMnNi quaternary HEAs. This potential is based on a previously developed potential for CrFeNi ternary alloys. The parameters to develop the potential were determined by fitting to experimental values, density functional theory (DFT) and thermodynamic calculations, to reproduce the main crystal characteristics, namely: the stability of the fcc phase, elastic constants, and stacking fault energy. Its applicability for the study of plastic deformation mechanisms was checked by calculations of behaviour of a $< 110>\left \{1111 \right \}$ edge dislocation in equiatomic quaternary CrFeMnNi alloy, as well as its less-complex subsystems (ternaries, binaries, and pure metals). The calculations were performed in the domain of temperatures between 0 and 900 K; smooth and stable glide of an edge dislocation and fcc phase stability in this temperature range was confirmed. This study demonstrates the suitability of the EAM-21 potential for the analysis of plasticity mechanisms and mechanical properties of CrFeMnNi HEAs.

cond-mat.mtrl-sci↗

Effects of the grain size and shape on the flow stress: A dislocation dynamics study

Dislocation dynamics simulation is used to investigate the effect of grain size and grain shape on the flow stress in model copper grains. We consider grains of 1.25-10 $μ$m size, three orientations (<135>, <100> and <111>) and three shapes (cube, plate and needles). Two types of periodic aggregates with one or four grains are simulated to investigate different dislocation flux at grain boundaries. It is shown that in all cases the flow stress varies linearly with the inverse of the square root of the grain size, with a proportionality factor varying strongly with the grain orientation and shape. Simulation results are discussed in the light of other simulation results and experimental observations. Finally, a simple model is proposed to account for the grain shape influence on the grain size effect.