arXiv · cond-mat/0609397
Thermal annealing study of swift heavy-ion irradiated zirconia
Abstract
Sintered samples of monoclinic zirconia (alpha-ZrO2) have been irradiated at room temperature with 6.0-GeV Pb ions in the electronic slowing down regime. X-ray diffraction (XRD) and micro-Raman spectroscopy measurements showed unambiguously that a transition to the 'metastable' tetragonal phase (beta-ZrO2) occurred at a fluence of 6.5x10^12 cm-2 for a large electronic stopping power value (approx 32.5 MeV $μ$m-1). At a lower fluence of 1.0x10^12 cm-2, no such phase transformation was detected. The back-transformation from beta- to alpha-ZrO2 induced by isothermal or isochronal thermal annealing was followed by XRD analysis. The back-transformation started at an onset temperature around 500 K and was completed by 973 K. Plots of the residual tetragonal phase fraction deduced from XRD measurements versus annealing temperature or time are analyzed with first- or second-order kinetic models. An activation energy close to 1 eV for the back-transformation process is derived either from isothermal annealing curves, using the so-called "cross-cut" method, or from the isochronal annealing curve, using a second-order kinetic law. Correlation with the thermal recovery of ion-induced paramagnetic centers monitored by EPR spectroscopy is discussed. Effects of crystallite size evolution and oxygen migration upon annealing are also addressed.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Jean-Marc Costantini, Andrée Kahn-Harari, Francois Beuneu, François Couvreur. 2006-09-18. Thermal annealing study of swift heavy-ion irradiated zirconia. https://doi.org/10.1063/1.2198927
Cite the original work for its findings. Save a collection to share your selection of sources.