Understanding Structural Representation in Foundation Models for Polymers

Abstract

From the relative scarcity of training data to the lack of standardized benchmarks, the development of foundation models for polymers face significant and multi-faceted challenges. At the core, many of these issues are tied directly to the structural representation of polymers and here, we present a new foundation model using a SMILES-based polymer graph representation. This approach allows representation of critical polymer architectural features and connectivity that are not available in other SMILES-based representations. The developed polymer foundation model exhibited excellent performance on 28 different benchmark datasets. Critical evaluation of the developed representation against other variations in control experiments reveals this approach to be a highly performant method of representing polymers in language-based foundation models. These control experiments also reveal a strong invariance of all SMILES representations, with many variations achieving state-of-the-art or near state-of-the-art performance, including those which are chemically or semantically invalid. Examination of error sources and attention maps for the evaluated representations corroborate the findings of the control experiments, showing that chemistry language models based on SMILES interpolate over all sequence space for prediction tasks, not only those of semantically valid inputs. Overall, this work highlights the importance of control experiments as a check on human-imposed assumptions that can limit rational design of both chemistry foundation models and their underlying structural representations.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Nathaniel H. Park, Eduardo Soares, Victor Y. Shirasuna, Tiffany J. Callahan, Sara Capponi, Emilio Vital Brazil. 2025-12-08. Understanding Structural Representation in Foundation Models for Polymers. https://arxiv.org/abs/2512.11881

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Slow Dynamics and the Geometry of Jammed Packings

Saddle points in the energy landscape of granular packings dominate the discrete steepest descent dynamics and ultimately determine the path that an out of mechanical equilibrium packing will follow and the resulting stable minimum that it will find. The saddle points that ultimately determine the resulting minima tend to be low-index saddle points. For models with an analytic energy landscape, such as the $p$-spin model, the steepest descent minimization path is affected by higher-index saddle points, which pull the system towards saddle points of decreasing index before arriving at the minima. Here, we examine the steepest descent minimization path of granular packings and compare them to the $p$-spin model. We show that the granular packing steepest descent minimization paths act like their smooth energy landscape counterparts and get attracted by saddle points. The index versus time curves for all models follow a shifted, stretched exponential. We further show that the shape parameter for the granular packings is unchanged when the energy landscape is modified to become analytic (Gaussian potential in a harmonic well) or non-local (Mari-Krzakala-Kurchan). The $p$-spin, on the other hand, has a significantly larger shape parameter. The reason is not due to the dimensionality, packing fraction, nonanalyticity, or the locality of the Hamiltonian of the models. The exact reason for the discrepancy in the shape parameter is \st{still} an unsolved mystery.

cond-mat.soft

A Phase-Field Study of Desiccation Crack Pattern Maturation under Drying-Wetting Cycles

The characteristic intersection angle of the desiccation crack relaxes from near \ang{90} toward \ang{120} under repeated drying--wetting cycles. However, the theoretical understanding of this relaxation is insufficient, especially the modeling of the drying--wetting cycles. Here we introduce a phase-field model of desiccation fracture, extending the model proposed in previous studies by adding crack healing and a scar effect left by past cracks. By repeating drying--wetting cycles in a finite element simulation, we find that the angle distribution develops a growing peak near \ang{120} as the cycle number increases, consistent with experiments. The standard deviation of the intersection angle from \ang{120} relaxes exponentially with a characteristic time of about 2.85 cycles. These results are consistent with experiments, except that the characteristic time is slightly smaller than the experimental value. Crack energy dominates the total energy and also relaxes exponentially with nearly the same characteristic cycle as the angle relaxation. This decay is driven mainly by a shortening of the effective crack length rather than a change in effective fracture toughness.

cond-mat.soft

Kinetics of ferritin crystal formation and melting in acoustically levitated droplets

Understanding protein crystallization pathways is essential for controlling crystallization in structural biology, materials science, and pharmaceutical applications. Classical nucleation theory does not fully capture crystallization processes for several proteins, including ferritin. Here, we combine acoustic levitation with small- and wide-angle X-ray scattering (SAXS and WAXS) to monitor ferritin crystallization in evaporating aqueous polyethylene glycol (PEG) solutions. Acoustic levitation rapidly drives the droplets through a broad range of protein and polymer concentrations, enabling time-resolved measurements of crystallization during evaporation. The scattering data show that ferritin crystals form during evaporation and subsequently lose their crystalline order upon further dehydration. Varying the PEG molecular weight switches between distinct crystallization pathways: one dominated by attractive protein-protein interactions and another dominated by repulsive interactions and excluded-volume effects. Furthermore, we find that lower molecular weight PEG (1000 g/mol) suppresses the dehydration-induced loss of crystalline order observed for higher molecular weight PEG (6000 g/mol), providing a simple strategy for improving protein crystal stability.

cond-mat.soft