Microstructure evolution and densification during spark plasma sintering of nanocrystalline W-5wt.%Ta alloy
Abstract
The present work reports the effect of Ta on densification and microstructure evolution during non-isothermal and spark plasma sintering of nanocrystalline W. Nanocrystalline W-5wt.%Ta alloy powder was synthesized using mechanical alloying. The nanocrystalline powder was characterized thoroughly using X-ray diffraction line profile analysis. Furthermore, the shrinkage behavior of nanocrystalline powder was investigated during non-isothermal sintering using dilatometry. Subsequently, the alloy powder was consolidated using spark plasma sintering up to 1600 {\deg}C. The role of Ta on stabilizing the microstructure during spark plasma sintering of nanocrystalline W was investigated in detail using electron backscatter diffraction. The average grain size of spark plasma sintered W-5wt.%Ta alloy was observed as 1.73 micron.
Explore related subjects
Keep this discovery
Ajeet K. Srivastav, Suresh Bandi, Abhishek Kumar, B. S. Murty. 2020-07-25. Microstructure evolution and densification during spark plasma sintering of nanocrystalline W-5wt.%Ta alloy. https://doi.org/10.1080/09500839.2020.1793010
Cite the original work for its findings. Save a collection to share your selection of sources.