Thermoelectric properties of Sr0.61Ba0.39Nb2O6-δ ceramics annealed in different oxygen-reduction conditions
Abstract
The thermoelectric properties of Sr0.61Ba0.39Nb2O6 ceramics, reduced in different conditions, were investigated in the temperature region from 323 K to 1073 K. The electrical transport behaviors of the samples are dominated by the thermal-activated polaron hopping, the Fermi glass behavior, and the Anderson localized behavior from low temperatures to high temperatures, respectively. The lattice thermal conductivity presents a plateau at high temperatures, indicating a glass-like thermal conduction behavior. Both the thermoelectric power factor and the thermal conductivity increase with the increasing degree of oxygen-reduction. Taking these two factors into account, the oxygen-reduction can still contribute to promoting the thermoelectric figure of merit. The highest ZT value (~0.19 at 1073 K) is obtained in the heaviest oxygen reduced sample.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Y. Li, J. Liu, C. L. Wang, W. B. Su, Y. H. Zhu, J. C. Li, L. M. Mei. 2014-04-02. Thermoelectric properties of Sr0.61Ba0.39Nb2O6-δ ceramics annealed in different oxygen-reduction conditions. https://doi.org/10.1088/1674-1056%2F24%2F4%2F047201
Cite the original work for its findings. Save a collection to share your selection of sources.