arXiv · 1303.1309
α-FeAs-free SmFeAsO1-xFx by low temperature sintering with slow cooling
Abstract
We obtained amorphous-FeAs-free SmFeAsO1-xFx using a low temperature sintering with slow cooling. SmFeAsO1-xFx is sintered at 980 °C for 40 hours and cooled slowly down to 600 °C. The low temperature sintering suppresses the formation of amorphous FeAs, and the slow cooling introduces much fluorine into SmFeAsO1-xFx. The superconductivity of this sample appears at 57.8 K and the superconducting volume fraction reaches 96 %. To study the change of fluorine concentration during the cooling process, samples are quenched by water at 950 °C, 900 °C, 850 °C, 800 °C, 750 °C and 700 °C. It is found that fluorine is substituted not only at the maximum heating temperature but also during the cooling process. The low temperature sintering with slow cooling is very effective to obtain a homogeneous SmFeAsO1-xFx with high fluorine concentration.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Masaya Fujioka, Saleem James Denholme, Toshinori Ozaki, Hiroyuki Okazaki, Keita Deguchi, Satoshi Demura, Hiroshi Hara, Tohru Watanabe, Hiroyuki Takeya, Takahide Yamaguchi, Hiroaki Kumakura, Yoshihiko Takano. 2013-08-07. α-FeAs-free SmFeAsO1-xFx by low temperature sintering with slow cooling. https://doi.org/10.7566/jpsj.82.094707
Cite the original work for its findings. Save a collection to share your selection of sources.